Follow
Marijana Majić Renjo
Marijana Majić Renjo
Incoming Control Manager at Koncar D&ST
Verified email at koncar-dst.hr
Title
Cited by
Cited by
Year
Enhancement of corrosion protection of AISI 304 stainless steel by nanostructured sol–gel TiO2 films
L Ćurković, HO Ćurković, S Salopek, MM Renjo, S Šegota
Corrosion science 77, 176-184, 2013
1782013
Vickers indentation fracture toughness of Y-TZP dental ceramics
D Ćorić, MM Renjo, L Ćurković
International Journal of Refractory Metals and Hard Materials 64, 14-19, 2017
892017
Indentation size effect of Y-TZP dental ceramics
MM Renjo, L Ćurković, S Štefančić, D Ćorić
Dental Materials 30 (12), e371-e376, 2014
502014
Statistical analysis of Vickers indentation fracture toughness of Y-TZP ceramics
D Ćorić, L Ćurković, M Majić Renjo
Transactions of FAMENA 41 (2), 1-16, 2017
312017
Thermal and rheological properties of water-based ferrofluids and their applicability as quenching media
J Župan, MM Renjo
Physics procedia 75, 1458-1467, 2015
222015
Rheological properties of aqueous alumina suspensions
M Majić Renjo, M Lalić, L Ćurković, G Matijašić
Materialwissenschaft und Werkstofftechnik 43 (11), 979-983, 2012
182012
Reverse indentation size effect of a duplex steel
MM Renjo, V Rede, L Curkovic
Kovove Materials 52, 299-304, 2014
162014
Erosion resistance of slip cast composite Al2O3-ZrO2 ceramics
MM Renjo, L Ćurković, K Grilec
Procedia Engineering 100, 1133-1140, 2015
152015
From eggshells biowaste to hydroxyapatite biomaterial: Von Eierschalen als Bioabfall bis zum Hydroxylapatit‐Biomaterial
L Ćurković, I Žmak, S Kurajica, ME Tonković, Z Šokčević, MM Renjo
Materialwissenschaft und Werkstofftechnik 48 (8), 797-802, 2017
122017
Application of different isotherm models on lead ions sorption onto electric furnace slag
L Ćurković, A Rastovčan-Mioč, M Majić, J Župan
The holistic approach to environment 1 (1), 13-18, 2011
122011
Critical evaluation of indentation fracture toughness measurements with Vickers indenter on yttria‐stabilized zirconia dental ceramics: Kritische Bewertung der mittels Vickers …
D Ćorić, M Majić Renjo, I Žmak
Materialwissenschaft und Werkstofftechnik 48 (8), 767-772, 2017
92017
Fracture toughness of alumina ceramics determined by vickers indentation technique
M Majić, L Ćurković
Materials Testing 54 (4), 228-232, 2012
92012
CO2 footprint for distribution oil immersed transformers according to ISO 14067: 2018
V Šerkinić, M Majić Renjo, V Ucović
Journal of Energy: Energija 69 (3), 0-0, 2020
72020
Poboljšanje svojstava Al2O3 keramike dodatkom nanočestica ZrO2
MM Renjo
Doktorski rad, Fakultet strojarstva i brodogradnje, Zagreb, 2016
62016
Effects of cold isostatic pressing and granule size distribution on the densification of alumina ceramics
L Ćurković, M Majić Renjo, D Ciglar
Materials Testing 57 (6), 495-498, 2015
62015
Investigation of glazed Y-TZP dental ceramics corrosion by surface roughness measurement
S Štefančić, L Ćurković, G Baršić, M Majić-Renjo, K Mehulić
Acta stomatologica Croatica: International journal of oral sciences and …, 2013
62013
Priprava stabilne suspenzije za lijevanje kompozitne keramike
I Andrić, L Ćurković
62012
Influence of surface roughness of alumina ceramics on indentation size
MM Renjo, L Ćurković, D Ćorić
Materials Testing 56 (1), 32-39, 2014
5*2014
Poboljšanje svojstava aluminijeve oksidne keramike dodatkom nanočestica cirkonijeva oksida
M Majić Renjo
doktorski rad, FSB, Zagreb, 2016
42016
Preparation of stable suspensions for slip casting of alumina-zirconia composite
M Majić Renjo, L Ćurković, I Andrić
International Scientific and Expert Conference" Technique, Education …, 2012
42012
The system can't perform the operation now. Try again later.
Articles 1–20