Effect of deep cryogenic treatment on the mechanical properties of tool steels
A Molinari, M Pellizzari, S Gialanella, G Straffelini, KH Stiasny
Journal of materials processing technology 118 (1-3), 350-355, 2001
6012001
Influence of shallow and deep cryogenic treatment on the residual state of stress of 4140 steel
D Senthilkumar, I Rajendran, M Pellizzari, J Siiriainen
Journal of Materials Processing Technology 211 (3), 396-401, 2011
1652011
Influence of load and temperature on the dry sliding behaviour of Al-based metal-matrix-composites against friction material
G Straffelini, M Pellizzari, A Molinari
Wear 256 (7-8), 754-763, 2004
1652004
Heat treatment and properties of a hot work tool steel fabricated by additive manufacturing
F Deirmina, N Peghini, B AlMangour, D Grzesiak, M Pellizzari
Materials Science and Engineering: A 753, 109-121, 2019
1592019
Tribological behaviour of hot rolling rolls
M Pellizzari, A Molinari, G Straffelini
Wear 259 (7-12), 1281-1289, 2005
1482005
Hot friction and wear behaviour of high speed steel and high chromium iron for rolls
M Pellizzari, D Cescato, MG De Flora
Wear 267 (1-4), 467-475, 2009
1362009
Thermal fatigue resistance of gas and plasma nitrided 41CrAlMo7 steel
M Pellizzari, A Molinari, G Straffelini
Materials Science and Engineering: A 352 (1-2), 186-194, 2003
1082003
Thermal fatigue resistance of plasma duplex-treated tool steel
M Pellizzari, A Molinari, G Straffelini
Surface and Coatings Technology 142, 1109-1115, 2001
1062001
High temperature wear and friction behaviour of nitrided, PVD-duplex and CVD coated tool steel against 6082 Al alloy
M Pellizzari
Wear 271 (9-10), 2089-2099, 2011
762011
Effect of sliding speed and contact pressure on the oxidative wear of austempered ductile iron
G Straffelini, M Pellizzari, L Maines
Wear 270 (9-10), 714-719, 2011
732011
Deep cryogenic treatment of cold work tool steel
M Pellizzari, A Molinari
Proceedings of 6th International Tooling Conference 1, 657-669, 2002
702002
Corrosion behaviour of a surface-treated AISI H11 hot work tool steel in molten aluminium alloy
A Molinari, M Pellizzari, G Straffelini, M Pirovano
Surface and coatings technology 126 (1), 31-38, 2000
682000
The phase stability in Cr–Ni and Cr–Mn duplex stainless steels
I Calliari, M Pellizzari, M Zanellato, E Ramous
Journal of materials science 46, 6916-6924, 2011
642011
Influence of processing parameters and particle size on the properties of hot work and high speed tool steels by spark plasma sintering
M Pellizzari, A Fedrizzi, M Zadra
Materials & Design 32 (4), 1796-1805, 2011
582011
Influence of laser hardening on the tribological properties of forged steel for hot rolls
M Pellizzari, MG De Flora
Wear 271 (9-10), 2402-2411, 2011
542011
Dry sliding wear of Cu–Be alloys
G Straffelini, L Maines, M Pellizzari, P Scardi
Wear 259 (1-6), 506-511, 2005
532005
Influence of deep cryogenic treatment on the thermal decomposition of Fe–C martensite
M Preciado, M Pellizzari
Journal of Materials Science 49, 8183-8191, 2014
522014
Feasibility of laser surface treatment of pearlitic and bainitic ductile irons for hot rolls
A Fernández-Vicente, M Pellizzari, JL Arias
Journal of Materials Processing Technology 212 (5), 989-1002, 2012
522012
Microstructural study and densification analysis of hot work tool steel matrix composites reinforced with TiB2 particles
A Fedrizzi, M Pellizzari, M Zadra, E Marin
Materials Characterization 86, 69-79, 2013
462013
Manufacturability of lattice structures fabricated by laser powder bed fusion: A novel biomedical application of the beta Ti-21S alloy
A Jam, A Du Plessis, C Lora, S Raghavendra, M Pellizzari, M Benedetti
Additive Manufacturing 50, 102556, 2022
412022